Low pressure casting is a development of permanent mold process. The mold is installed on a sealed furnace containing molten metal. The riser tube connects the bottom of the mold to the molten metal bath. The chamber containing the molten metal is pressured (typically 20-100kPa), and the metal is forced up into the mold..Low pressure casting can perform with Aluminium, zinc, copper alloys. Low pressure casting offers high yields in excess of 90% as risers and runners are limited, also reducing fettling and trimming costs. Pore free castings are obtainable and machine size will limit the size of castings.
As a low pressure casting parts designer, manufacturer, supplier in Ningbo China, Our Aluminium casting foundry have more than 10 years experience with low pressure castings, sells the Aluminium products all over the world. Our low pressure casting parts include low pressure casting gear housing, low pressure casting case, low pressure casting pipe fittings, low pressure casting cylinder housing, low pressure casting engine piston, low pressure casting cylinder parts, custom low pressure casting part, low pressure casting wheel, cast Aluminium parts, low pressure casting s cylinder head, low pressure casting s industry parts, low pressure casting cylinder block, low pressure casting cylinder cover, low pressure castings pump body, low pressure castings cylinder body, low pressure casting valve body, low pressure casting cylinder cover hood etc.
Production
-Our low pressure casting s foundry is specialized in manufacturing low pressure casting parts, together with full capacity of CNC machining for sand castings.
-Tooling design & manufacture for low pressure casting s
-Design capability for low pressure casting s parts
Universal material for low pressure casting s: A356-T6, AlMg35, A413 etc.
-low pressure casting s heat treatment with F, T1, T2, T4, T6, T5, T651
-excellent surface treatment technique for low pressure casting Aluminium part include: alodine, anodizing, powder coating, plating, mirror polishing, Nickel plate, chromate plating, zinc plating, gold finish, matt polishing, e-coating, wet painting, passivation and etc.
Here below are the low pressure casting material comparison from different country :
MATERIAL COMPARISON TABLE for ALUMIINUM LOW PRESSURE CASTING PARTS |
|||||||
China |
USA |
|
UK |
France |
Germany |
Japan |
ISO |
GB |
ASTM |
ANSI |
BS |
NF |
DIN |
JIS |
|
ZL101 |
A03560 |
356 |
\ |
A-S7C |
G-AlSi7Mg |
AC4C |
AlSi7Mg |
ZL101A |
A13560 |
A356.0 |
\ |
\ |
\ |
\ |
AlSi7MgA |
ZL102 |
A14130 |
A413 |
LM20 |
A-S13 |
G-AlSi12 |
AC3A |
AlSi12 |
ZL104 |
A03600 |
A360 |
LM9 |
A-S9G |
G-AlSi10Mg |
AC4A |
AlSi9Mg |
ZL105 |
A035500 |
A355 |
LM16 |
\ |
G-AlSi5Cu |
AC4D |
AlSi5Cu1Mg |
ZL106 |
A0328 |
328.0 |
LM-24 |
\ |
G-ALSI8CU3 |
AC4B |
Al8Cu1Mg |
ZL115 |
\ |
\ |
\ |
\ |
\ |
\ |
Al5Zn1Mg |
ZL116 |
\ |
\ |
\ |
\ |
\ |
\ |
AlSi8MgBE |
ZL201 |
\ |
\ |
\ |
A-U5GT |
G-AlCu4TiMg |
\ |
AlCu4MgTi |
ZL202 |
A03600 |
A360.0 |
\ |
A-U8S |
\ |
\ |
AlCu10 |
ZL203 |
A029500 |
295.0 |
\ |
A-U5GT |
G-AlCu4Ti |
\ |
Al-Cu4MgTi |
ZL301 |
A05200 |
520.0 |
LM10 |
|
G-AlMg10 |
AC7B |
AlMg10 |
ZL303 |
\ |
\ |
\ |
\ |
\ |
\ |
AlMg5Si1 |
ZL305 |
\ |
\ |
\ |
\ |
\ |
\ |
AlMg8Zn1 |
ZL401 |
\ |
\ |
\ |
\ |
\ |
\ |
AlZn11Si7 |
ZL402 |
A071200 |
712.2 |
\ |
A-Z5C |
\ |
\ |
AlZn6Mg |
Our company quality controls are carried out on incoming materials, production processes, finished products and services in compliance with the regulations of ISO9000:2008.
Delivery
-For our new customer, we will arrange the contact review meeting to confirm the stable delivery time after receiving the purchase order, The delivery time we advise is reasonable and precision.
-we will produce some extra goods in our warehouse for stock each time, so anytime you need the delivery is possible.
-If the production meet resistance and may influence the delivery, we will inform to you in the first time. And we take the most efficiency plan to solve the problem.
Any of your comments and queries will be highly appreciated. Thanks!